Nickel Alloy Sheet & Plate 201, also known as Nickel Alloy 201, is a high-purity nickel alloy with excellent resistance to oxidation and corrosion, particularly in reducing environments. Nickel 201 is commonly designated by the material number UNS N02201.This designation helps to standardise the alloy and its properties, ensuring that it meets specific criteria for applications requiring high-purity nickel with excellent corrosion resistance.
3/16″ | 1/4″ | 3/8″ | 1/2″ | 5/8″ | 3/4″ | 1″ |
---|---|---|---|---|---|---|
4.8mm | 6.3mm | 9.5mm | 12.7mm | 15.9mm | 19.0mm | 25.4mm |
Country | Standard | Grade |
---|---|---|
USA | ASTM | Nickel 201 |
Europe | EN | Ni 99.2 |
Germany | DIN | 2.4061 |
Japan | JIS | NW 2200 |
China | GB | Ni99.2 |
India | IS | 2205 |
South Korea | KS | N601 |
Element | Percentage (%) |
---|---|
Nickel (Ni) | 99.0 – 99.5 |
Carbon (C) | ≤ 0.02 |
Manganese (Mn) | ≤ 0.35 |
Silicon (Si) | ≤ 0.35 |
Sulfur (S) | ≤ 0.01 |
Iron (Fe) | ≤ 0.40 |
Copper (Cu) | ≤ 0.25 |
Property | Value |
---|---|
Density | 8.90 g/cm³ |
Melting Point | 1455°C (2651°F) |
Thermal Conductivity | 90 W/m·K |
Electrical Resistivity | 6.99 µΩ·cm |
Modulus of Elasticity | 207 GPa (30 x 10⁶ psi) |
Poisson’s Ratio | 0.31 |
Property | Value |
---|---|
Tensile Strength | 50 – 70 ksi (345 – 480 MPa) |
Yield Strength | 30 – 50 ksi (205 – 345 MPa) |
Elongation | 30 – 40% (in 2 inches) |
Hardness | 70 – 90 HRB |
Modulus of Elasticity | 207 GPa (30 x 10⁶ psi) |
Fatigue Strength | Varies with application |
For more information or to request a quote, contact us today to discuss how Nickel Alloy Sheet & Plate 201 can meet your specific project needs.